What is angle-resolved XPS?

Analysis of a thin oxide film on a metal at near-normal and near-grazing collection angles could produce spectra with a larger relative intensity of the oxide peak at the near-grazing emission angle.

The information depth for XPS is a few nanometers, depending upon the kinetic energy of the electrons and the material being analyzed. Angle-resolved XPS (ARXPS), however, is a technique that varies the emission angle at which the electrons are collected, thereby enabling electron detection from different depths. ARXPS provides information about the thickness and composition of ultra-thin films. Such measurements are non-destructive, unlike sputter profiling.

Analysis of a thin oxide film on a metal at near-normal and near-grazing collection angles could produce spectra with a larger relative intensity of the oxide peak at the near-grazing emission angle.

Three major reasons why angle-resolved XPS is useful

  • It can be applied to films that are too thin to be analyzed by conventional depth profiling techniques.
  • It can be applied to films that are irretrievably damaged by sputtering (e.g., polymers).
  • It is non-destructive and can provide chemical state information, unlike methods based upon sputtering.

Angle-resolved XPS measurements provide the following information:

  • Ordering of layers in an ultra-thin film.
  • Thickness of layers
  • Distribution of elements and chemical states within the film (depth profile reconstruction).

Angle-resolved XPS data acquisition

Angle-resolved XPS experiments are undertaken in a serial manner, by limiting the angular acceptance of the analyzer and stepping through a range of angles in turn. This is usually undertaken by tilting the sample with respect to the analyzer.

Angle-resolved XPS data is collected using a series of sample tilt angles.
Angle-resolved XPS data is collected using a series of sample tilt angles.

Products

仪器卡片原件样式表

Nexsa G2 XPS

  • 微焦点 X 射线源
  • 独特的多技术选项
  • 用于单原子和簇离子深度剖析的双模式离子源

K-Alpha XPS

  • 高分辨率 XPS
  • 快速、高效、自动化的工作流程
  • 用于深度剖析的离子源

ESCALAB QXi XPS

  • 高光谱分辨率
  • 多技术表面分析
  • 丰富的样品制备和扩展选项
用于将 H2 样式更改为具有 em-h2-header 类 p 的样式表

Contact us