Primary XPS region: Pb4f
Overlapping regions: N/A
Binding energies of common chemical states:
| Chemical state | Binding energy Pb4f7/2/eV |
|---|---|
| Pb metal | 136.9 |
| PbO2 | 137.8 |
| Pb3O4 | 138.4 |
| Pb native oxide | 138.4 |
| 2PbCO3.Pb(OH)2 | 138.4 |
| Pb palmitate | 138.4 |
| Pb azelate | 138.4 |
Native oxide referenced to Pb metal. All others charge referenced to adventitious C1s peak at 284.8eV.
N/A


About This ElementSymbol: Pb
Date of Discovery: known to the ancients
Name Origin: Latin plumbum
Appearance: bluish-white
Discoverer: unknown
Obtained From: galena
Melting Point: 600.1 K
Boiling Point: 2022 K
Density[kg/m3]: 11.340
Molar Volume: 18.26 × 10-6 m3/mol
Protons/Electrons: 82
Neutrons: 125
Shell Structure: 2,8,18,32,18,4
Electron Configuration: [Xe]4f145d106s26p2
Oxidation State: 4,2
Crystal Structure: cubic
This blue-white metal is soft and malleable. A poor conductor of electricity, lead is resistant to corrosion and very dense. Lead derives its symbol Pb from the Latin word plumbum, meaning “liquid silver.” Prolonged exposure to lead causes neurological damage as well as renal disease, cardiovascular effects, and reproductive toxicity. Although the harmful effects of lead have been recognized as early as 2000 BC, it has been used throughout history for plumbing and ammunition. Recently, lead has been used in storage batteries, paints, petrol, and sound absorbance materials, although these uses are being phased out due to health and environmental effects.